Customization: | Available |
---|---|
Feature: | Long Time Materials, High Temperature Resistant |
Refractoriness (℃): | 1770< Refractoriness< 2000 |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
No. | A-45 | A-60 | A-70 | A-75 | A-80 | A-90 | |
Dry Density (g/cm3) ≥ | 2.3 | 2.5 | 2.6 | 2.65 | 2.7 | 3 | |
Chemical (%) | Al2O3≥ | 45 | 60 | 70 | 75 | 80 | 90 |
ZrO2 | -- | -- | -- | -- | -- | -- | |
Modulus of Rupture(Mpa) | 110oC×24h≥ | 5 | 8 | 9 | 9 | 10 | 12 |
1500oC×3h≥ | 8(1350oC) | 10 (1450oC×3h) | 12 | 15 | |||
Compressive Strength(Mpa) | 110oC×24h≥ | 30 | 40 | 40 | 45 | 45 | 60 |
1450oC×3h≥ | 60 | 80 | 80 | 85 | 90 | 85 | |
Linear Dimensional Change After Fired (1500oC×3h)%≤ | ±0.5 | ±0.5 | ±0.5 | ±0.5 | ±0.5 | ±0.5 | |
1350oC×3h | 1450oC×3h | 1450oC×3h | 1450oC×3h | ||||
Refractoriness(oC)≥ | 1710 | 1740 | 1790 | 1790 | 1790 | 1790 | |
Working Temp(oC) | 1450 | 1450 | 1500 | 1550 | 1600 | 1650 |